ASTM A384/A384M-07(2013)
Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies
3 стр.
Заменен
Электронный (pdf)Печатное издание
84.24 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
25.220.20 Surface. Including anodization, conversion coating, thermal spraying, etc. / Обработка поверхности. Включая анодирование, покрытия, химически взаимодействующие с подложкой, термораспыление и т.д.
Сборник (ASTM):
01.06 Coated Steel Products / Изделия из облицовочной стали
Тематика:
Steel--Structural, Tubes, Plate, Coated
Описание
Реферат

This specification deals with safeguarding against warpage and distortion during hot-dip galvanizing of steel assemblies. Common distorted and warped members of assemblies are sheets or plates assembled by welding or riveting. The following can cause warpage and distortion: use of nonsymmetrical sections such as channels; use of checkered plate; not properly vented overlapping joint for two pieces of steel; and too large assembly for a particular galvanizing kettle. Suggested corrections for panel fabrication are detailed.

Область применения

1.1 Steel assemblies and subassemblies fabricated by welding, such as composite structural members, sash, weldments, etc., that are to be hot-dip galvanized after fabrication, are subject to warpage and distortion of the material due to the heating and cooling integral to the galvanizing operation, particularly when it is necessary for the assembly to be dipped more than once to coat the entire surface.

1.2 This specification is applicable in either inch pounds or SI units. Inch pounds and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in parentheses.

Ключевые слова:
coatings-zinc; galvanized coatings; steel products-metallic coated; zinc coatings-steel products