(812) 309-78-59
(495) 223-46-76
ASTM B443-00(2009)
Standard Specification for Nickel-Chromium-Molybdenum-Columbium Alloy (UNS N06625) and Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219)* Plate, Sheet, and Strip
8 стр.
Заменен
Электронный (pdf)Печатное издание
96.72 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
77.150.40 Nickel and chromium products / Продукция из никеля и хрома
Сборник (ASTM):
02.04 Nonferrous Metals – Nickel, Titanium, Lead, Tin, Zinc, Zirconium, Precious, Reactive, Refractory Metals and Alloys: Materials for Thermostats, Electrical Heating and Resistance Contact, and Connectors / Цветные металлы - Никель, Кобальт, Свинец, Олово, Цинк, Кадмий, Драгоценные металлы, химически активные металлы, Тугоплавкие металлы и сплавы, Материалы для Термостатов, Электронагревательных приборов, Контактов, Соединительные устройств
Тематика:
Other Nonferrous Metals
Описание
Реферат

This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS No. N06625) and nickel-chromium-molybdenum-silicon alloy (UNS No. N06219) plates, sheets, and strips. N06625 alloys shall be furnished in two grades of different heat treatment conditions, namely: Grade 1 (annealed); and Grade 2 (solution annealed). N06219 alloys, on the other hand, shall be furnished in solution annealed condition only. Materials shall be sampled prepared, and tested accordingly to examine their conformance to dimensional (thickness, weight, width, diameter, length, straightness, edges, squareness, and flatness), mechanical (tensile and yield strengths, and elongation), and chemical composition requirements.

Область применения

1.1 This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS N06625) and nickel-chromium-molybdenum-silicon alloy (UNS N06219)* plate, sheet, and strip.

1.1.1 Alloy UNS N06625 products are furnished in two grades of different heat-treated conditions:

1.1.1.1 Grade 1 (Annealed)Material is normally employed in service temperatures up to 1100°F (593°C).

1.1.1.2 Grade 2 (Solution Annealed)Material is normally employed in service temperatures above 1100°F (593°C) when resistance to creep and rupture is required.

Note 1—Hot-working or reannealing may change properties significantly, depending on working history and temperatures.

1.1.2 Alloy UNS N06219 is supplied in solution annealed condition only.

1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
UNS N06219; UNS N06625; plate; sheet; strip; Nickel-chromium-molybdenum-silicon alloys--specifications; Rolled nickel-chromium-molybdenum-columbium alloys; Udimet alloy; UNS N06219 (Ni-Cr-Mo-Si alloy, Nicrofer 6219Si); UNS N06625 (Ni-Cr alloy, Inconel 625); Nickel alloy plate/sheet/strip--specifications; Nickel-chromium alloys--specifications; Nickel-chromium-molybdenum-columbium alloys--specifications