ASTM C1366-97
Standard Test Method for Tensile Strength of Monolithic Advanced Ceramics at Elevated Temperatures
27 стр.
Заменен
Печатное изданиеЭлектронный (pdf)
134.16 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
81.060.30 Advanced ceramics / Высококачественная керамика
Сборник (ASTM):
15.01 Refractories, Activated Carbon; Advanced Ceramics / Огнеупорные материалы; Активированный уголь, Высококачественная керамика
Тематика:
Glass, Ceramics
Описание
Область применения

1.1 This test method covers the determination of tensile strength under uniaxial loading of monolithic advanced ceramics at elevated temperatures. This test method addresses, but is not restricted to, various suggested test specimen geometries as listed in the appendix. In addition, specimen fabrication methods, testing modes (load displacement, or strain control), testing rates (load rate, stress rate, displacement rate, or strain rate), allowable bending, and data collection and reporting procedures are addressed. Tensile strength as used in this test method refers to the tensile strength obtained under uniaxial loading.

Ключевые слова: