ASTM D3897-18
Standard Test Method for Calculation of Basicity of Chrome Tanning Liquors
2 стр.
Действует
Электронный (pdf)Печатное издание
68.64 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
59.140.10 Processes and auxiliary materials / Процессы и вспомогательные материалы
Сборник (ASTM):
15.04 Soaps and Other Detergents; Polishes; Leather; Resilient Floor Coverings / Мыло и другие моющие средства; Полировальные материалы; Кожа; Эластичные покрытия для полов
Тематика:
Leather
Описание
Значение и использование

3.1 Basicity is a ratio. In any chromic salt solution, the electrovalence of the chromium (+3) is satisfied by the hydroxyl ions and by acid ions. The extent to which this electravalence is satisfied by the hydroxyl ions, expressed as a percentage, is the basicity. The basicity of a chrome tanning liquid is closely related to the tanning behavior of the solution.

Область применения

1.1 This test method is intended to show how the results of the chromium analysis (Test Methods D3898 or D6019) and the acidity determination (Test Method D3913) can be combined to permit calculation of the basicity of a chrome tanning liquor.

1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Ключевые слова:
basicity; chrome tanning liquor; Schorlemmer;