(812) 309-78-59
(495) 223-46-76
ASTM D6558-00a(2005)
Standard Test Method for Determination of TGA CO2 Reactivity of Baked Carbon Anodes and Cathode Blocks
5 стр.
Заменен
Электронный (pdf)Печатное издание
96.72 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
77.020 Production of metals / Производство металлов
Сборник (ASTM):
05.03 Petroleum Products, Liquid Fuels, and Lubricants (III): D6138–D6971 / Нефтепродукты, жидкое топливо и смазочные материалы (III): D6138–D6971
Тематика:
Petroleum
Описание
Значение и использование

The CO2 reactivity rates are used to quantify the tendency of a carbon artifact to react with carbon dioxide. Carbon consumed by these unwanted side reactions is unavailable for the primary reactions of reducing alumina to the primary metal. CO2 dusting rates are used to quantify the tendency of the coke aggregate or binder coke of a carbon artifact to selectively react with these gases. Preferential attack of the binder coke or coke aggregate of a carbon artifact by these gases causes some carbon to fall off or dust, making the carbon unavailable for the primary reaction of reducing alumina and, more importantly, reducing the efficiency of the aluminum reduction cell.

Comparison of CO2 reactivity and dusting rates is useful in selecting raw materials for the manufacture of commercial anodes for specific smelting technologies in the aluminum reduction industry.

CO2 reactivity rates are used for evaluating effectiveness and beneficiation processes or for research purposes.

Область применения

1.1 This test method covers the thermogravimetric (TGA) determination of CO2 reactivity and dusting of shaped carbon anodes and cathode blocks used in the aluminum reduction industry. The apparatus selection covers a significant variety of types with various thermal conditions, sample size capability, materials of construction, and procedures for determining the mass loss and subsequent rate of reaction. This test method standardizes the variables of sample dimensions, reaction temperature, gas velocity over the exposed surfaces, and reaction time such that results obtained on different apparatuses are correlatable.

1.2 &solely-SI-units;

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
anode; cathode block; CO2 reactivity; dusting