(812) 309-78-59
(495) 223-46-76
ASTM D6933-08
Standard Test Method for Oversized Particles in Emulsified Asphalts (Sieve Test)
2 стр.
Заменен
Электронный (pdf)Печатное издание
84.24 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
93.080.20 Road. Including asphalts, road pavements, etc. / Дорожно-строительные материалы. Включая асфальт, дорожные покрытия и т.д.
Сборник (ASTM):
04.03 Road and Paving Materials; Vehicle–Pavement Systems / Материалы для покрытия и мощения дорог, Дорожно-транспортные системы
Тематика:
Road & Paving
Описание
Значение и использование

The retention of an excessive amount of particles on the sieve indicates that problems may occur in handling and application of the material. Particles of asphalt retained on the sieve often are caused by agglomeration of the dispersed phase. Storage, pumping, handling, and temperature can all contribute to the formation of particles. Contamination from the tank, transport, or hose are other factors affecting particle formation.Область применения

1.1 This test method covers the degree to which an emulsified asphalt may contain particles of asphalt or other discreet solids retained on a 850-μm mesh sieve.

1.2 This test method does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
asphalt; asphalt emulsion; cationic emulsified asphalt; emulsified asphalt; oversized particles; sieve test; Cationic emulsified asphalt; Emulsified asphalt; Sieve analysis--asphalts