(812) 309-78-59
(495) 223-46-76
ASTM D7460-10
Standard Test Method for Determining Fatigue Failure of Compacted Asphalt Concrete Subjected to Repeated Flexural Bending (Withdrawn 2019)
14 стр.
Отменен
Электронный (pdf)Печатное издание
107.64 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
91.100.50 Binders. Including geomembranes, asphalts for buildings, etc. / Связующие вещества. Уплотнители. Включая геомембраны, строительный асфальт и т.д.
Сборник (ASTM):
04.03 Road and Paving Materials; Vehicle–Pavement Systems / Материалы для покрытия и мощения дорог, Дорожно-транспортные системы
Тематика:
Road & Paving
Описание
Причина отменыThis test method provided procedures for determining a unique failure point for estimating the fatigue life of 380 mm (14.96 in.) long by 50 mm (1.97 in.) thick by 63 mm (2.48 in.) wide asphalt concrete beam specimens sawed from laboratory or field compacted asphalt concrete, which are subjected to repeated flexural bending.

Formerly under the jurisdiction of Committee D04 on Road and Paving Materials, this test method was withdrawn in June 2019 in accordance with section 10.6.3 of the Regulations Governing ASTM Technical Committees, which requires that standards shall be updated by the end of the eighth year since the last approval date.

Значение и использование

The laboratory fatigue life determined by this standard for beam specimens have been used to estimate the fatigue life of asphalt concrete pavement layers under repeated traffic loading. Although the field performance of asphalt concrete is impacted by many factors (traffic variation, speed, and wander; climate variation; rest periods between loads; aging; etc.), it has been more accurately predicted when laboratory properties are known along with an estimate of the strain level induced at the layer depth by the traffic wheel load traveling over the pavement.

Note 1—The quality of the results produced by this standard are dependent on the competence of the personnel performing the procedure and the capability, calibration, and maintenance of the equipment used. Agencies that meet the criteria of Specification D3666 are generally considered capable of competent and objective testing/sampling/inspection/etc. Users of this standard are cautioned that compliance with Specification D3666 alone does not completely assure reliable results. Reliable results depend on many factors; following the suggestions of Specification D3666 or some similar acceptable guideline provides a means of evaluating and controlling some of those factors.

Область применения

1.1 This test method provides procedures for determining a unique failure point for estimating the fatigue life of 380 mm (14.96 in.) long by 50 mm (1.97 in.) thick by 63 mm (2.48 in.) wide asphalt concrete beam specimens sawed from laboratory or field compacted asphalt concrete, which are subjected to repeated flexural bending.

1.2 The between-laboratory reproducibility of this test method is being determined and will be available on or before June 2013. Therefore, this test method should not be used for acceptance or rejection of a material for purchasing purposes.

1.3 The text of this standard references notes and footnotes which provide explanatory material. These notes and footnotes (excluding those in tables and figures) shall not be considered as requirements of the standard.

1.4 UnitsThe values stated in SI units are to be regarded as standard. Other units of measurement included in this standard are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
asphalt concrete fatigue; asphalt concrete flexural testing; asphalt concrete stiffness; asphalt concrete tensile testing; fatigue life; flexural bending; Asphalt concrete; Fatigue life; Flexural testing