ASTM G19-04
Standard Test Method for Disbonding Characteristics of Pipeline Coatings by Direct Soil Burial (Withdrawn 2010)
4 стр.
Отменен
Электронный (pdf)Печатное издание
84.24 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
87.040 Paints. Including coating powders, paint coatings and protective paint systems / Краски и лаки. Включая порошки для нанесения покрытий, лакокрасочные покрытия и системы защитной окраски
Сборник (ASTM):
06.02 Paint –– Products and Applications; Protective Coatings; Pipeline Coatings / Красители – Продукты и их применение; Защитные покрытия; Покрытия для трубопровода
Тематика:
Paints & Related Coatings
Описание
Причина отмены

This test method describes the determination of the relative disbonding characteristics of damaged coatings on steel pipe by cathodic protection potentials in direct soil burial. This test method is intended to apply to the testing of all types of nonmetallic pipeline coatings and tapes including thermoplastics, thermoset, and bituminous materials.

Formerly under the jurisdiction of Committee D01 on Paint and Related Coatings, Materials, and Applications this test method was withdrawn in June 2010. This standard is being withdrawn without replacement due to its limited use by industry.

Значение и использование

Coated pipe is seldom, if ever, buried without some damage to the coating. Hence, an actual soil-burial test can contribute significant data, provided the method of testing is controlled and the test specimen monitored and the relationship between the area disbonded, the current demand, and the mode of failure is fully understood.

Means are provided for measuring and following the electrical potential and current flow and relating these data to the final measurement of disbonded area.

Область применения

1.1 This test method describes the determination of the relative disbonding characteristics of damaged coatings on steel pipe by cathodic protection potentials in direct soil burial. This test method is intended to apply to the testing of all types of nonmetallic pipeline coatings and tapes including thermoplastics, thermoset, and bituminous materials.

1.2 Results may vary widely when test sites are in different geographical areas of the country, and even in different localities.

1.3 This test method is limited to nonconducting, or nonmetallic pipe coatings and is not applicable to conducting materials such as zinc coatings on steel pipe.

1.4 The values stated in SI units to three significant decimals are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
cathodic disbonding; pipeline coatings; soil burial