SAE AMS5843G
Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
Заменен
Печатная копияПечатное изданиеЭлектронный (pdf)
124.20 $ (включая НДС 20%)
Разработчик:
Зарубежные/Группа SAE/SAE
Тематика:
MetallurgyHeat treatmentHeat resistant materialsCobalt alloysNickel alloysNonferrous alloysMaterials properties
Описание
This specification covers a high strength, corrosion and heat-resistant cobalt-nickel-chromium alloy in the form of bars (see 8.2).