(812) 309-78-59
(495) 223-46-76
ASTM E561-98
Standard Practice for R-Curve Determination
13 стр.
Заменен
Электронный (pdf)Печатное издание
104.52 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
77.040.10 Mechanical testing of metals / Механические испытания металлов
Сборник (ASTM):
03.01 Metals -- Mechanical Testing; Elevated and Low-Temperature Tests; Metallography / Металлы - Механические испытания, Испытания при высоких и низких температурах, Металлография
Тематика:
Fatigue & Fracture
Описание
Область применения

1.1 This practice covers the determination of resistance to fracturing of metallic materials by R-curves using either the center-cracked tension panel M(T), the compact specimen C(T), or the crack-line-wedge-loaded specimen C(W), to deliver applied stress intensity factor, K, to the material. An -curve is a continuous record of toughness development in terms of KR plotted against crack extension in the material as a crack is driven under a continuously increased stress intensity factor, .

1.2 Materials that can be tested for -curve development are not limited by strength, thickness, or toughness, so long as specimens are of sufficient size to remain predominantly elastic throughout the duration of the test.

1.3 Specimens of standard proportions are required, but size is variable, to be adjusted for yield strength and toughness of the materials.

1.4 Only three of the many possible specimen types that could be used to develop -curves are covered in this practice.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
Fracture testing; sharp-notch tension, on high-strength thick aluminum and magnesium alloy; products, with cylindrical specimens, practice,; R-curves; fracture resistance of metallic materials, practice