(812) 309-78-59
(495) 223-46-76
ASTM D6095-05
Standard Test Method for Volume Resistivity for Extruded Crosslinked and Thermoplastic Semiconducting Conductor and Insulation Shielding Materials
3 стр.
Заменен
Электронный (pdf)Печатное издание
84.24 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
29.045 Semiconducting materials / Полупроводниковые материалы29.060.01 Electrical wires and cables in general / Электрические провода и кабели в целом
Сборник (ASTM):
10.02 Electrical Insulation (II): D2519–latest / Электрическая изоляция (II): с D2518 и далее
Тематика:
Electrical Insulating Materials
Описание
Область применения

1.1 This test method covers the procedure for determining the volume resistivity, measured longitudinally, of extruded crosslinked and thermoplastic semiconducting, conductor and insulation shields for wire and cable.

1.2 Whenever two sets of values are presented, in different units, the values in the first set are the standard, while those in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. For a specific hazard statement, see .

1.3 In common practice the conductor shield is often referred to as the strand shield.

1.4 While technically the volume resistivity in this test method is a longitudinal measurement of volume resistivity, in the wire and cable industry the word longitudinal is not used. This longitudinal measurement of volume resistivity will be referred to as "volume resistivity" throughout this standard.

Ключевые слова:
conductor shield; conductor shielding material; insulation shield; insulation shielding material; moderately conductive; semiconducting shielding materials; semiconducting shields; volume resistivity of shielding materials