(812) 309-78-59
(495) 223-46-76
ASTM D2149-13
Standard Test Method for Permittivity (Dielectric Constant) And Dissipation Factor Of Solid Ceramic Dielectrics At Frequencies To 10 MHz And Temperatures To 500°C
4 стр.
Заменен
Электронный (pdf)Печатное издание
84.24 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
29.035.30 Glass and ceramic insulating materials / Стеклянные и керамические изоляционные материалы
Сборник (ASTM):
10.01 Electrical Insulation (I): D69–D2484 / Электрическая изоляция (I): D69-D2484
Тематика:
Electrical Insulating Materials
Описание
Значение и использование

4.1 Permittivity and dissipation factor are sensitive to changes in chemical composition, impurities, and homogeneity. Measurement of these properties is, therefore, useful for quality control and for determining the effect of environments such as moisture, heat, or radiation.

Область применения

1.1 This test method covers the determination of the relative permittivity (dielectric constant) and dissipation factor of solid dielectrics from 50 Hz to 10 MHz over a range of temperatures from −80 to 500°C.2 ,3 Two procedures are included as follows:

1.1.1 Procedure A—Using Micrometer Electrode.

1.1.2 Procedure B—Using Precision Capacitor.

Note 1In common usage the word “relative” is frequently dropped.

1.2 This standard does not purport to address the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
dielectric constants; dissipation factors; micrometer electrodes; permittivities; precision capacitors; relative permittivities