ASTM D6723-02
Standard Test Method for Determining the Fracture Properties of Asphalt Binder in Direct Tension (DT) (Withdrawn 2011)
12 стр.
Заменен
Печатное изданиеЭлектронный (pdf)
107.64 $ (включая НДС 20%)
Разработчик:
Зарубежные/ASTM
ICS:
93.080.20 Road. Including asphalts, road pavements, etc. / Дорожно-строительные материалы. Включая асфальт, дорожные покрытия и т.д.91.100.50 Binders. Including geomembranes, asphalts for buildings, etc. / Связующие вещества. Уплотнители. Включая геомембраны, строительный асфальт и т.д.
Сборник (ASTM):
04.03 Road and Paving Materials; Vehicle–Pavement Systems / Материалы для покрытия и мощения дорог, Дорожно-транспортные системы
Тематика:
Road & Paving
Описание
Причина отмены

Formerly under the jurisdiction of Committee D04 on Road and Paving Materials, this Test Method was withdrawn in 2011 in accordance with section 10.5.3.1 of the Regulations Governing ASTM Technical Committees, which requires that standards shall be updated by the end of the eighth year since the last approval date.

Значение и использование

Stress at failure is used in a mechanistic pavement cracking model to compute critical cracking temperature. The procedure to compute critical cracking temperature is described in Practice D 6521. The critical cracking temperature is then used in specifying the low temperature grade of asphalt binder in accordance with Specification D 6373.

The test method is designed to measure the strength of the asphalt binder at the critical cracking temperature. The asphalt binder has limited ability to resist stress without cracking. In the asphalt binder Specification D 6373, failure stress is used to determine the critical cracking temperature.

For evaluating an asphalt binder for conformance to Specification D 6373, the elongation rate of the gage section is 1.0 mm/min and the test temperature is selected from Table number 1 of Specification D 6373 according to the grade of asphalt binder. Other rates of elongation and test temperatures may be used to test asphalt binders.

Область применения

1.1 This test method covers the determination of the failure strain and failure stress of asphalt binders by means of a direct tension test. It can be used with unaged material or with material aged using Test Method D 2872 (RTFOT), Practice D 6521 (PAV), or AASHTO T240 (RTFOT) and AASHTO PP1 (PAV). The test apparatus is designed for testing within the temperature range from +6 to -36°C.

1.2 This test method is limited to asphalt binders containing particulate material having dimensions less than 250 μm.

1.3 The values stated in SI units are to be regarded as the standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Ключевые слова:
asphalt binder; direct tension; failure; failure strain; fracture; thermal cracking