This specification covers ductile iron castings for use in pressure containing paper mill dryer rolls. The castings shall be stress relieved through heat treatment and shall undergo chemical analysis and conform to the required chemical composition in total carbon, silicon, phosphorus, and sulfur. Tension test specimens shall be obtained from test coupons poured from the same iron as the castings represented and shall conform to the prescribed mechanical properties such as yield strength, tensile strength, and elongation. Hardness test shall be conducted on the material and shall meet the required Brinell hardness value.
Область применения1.1 This specification covers ductile iron castings for use in pressure containing paper mill dryer rolls at temperatures up to 450F [230C].
1.2 No precise quantitative relationship can be stated between the properties of the iron in various locations of the same casting or between the properties of a casting and those of a test specimen cast from the same iron (see ).
1.3 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.