This specification covers a group of common requirements which shall apply to tin mill products. The steel shall be made by the open-hearth, electric-furnace, or basic-oxygen process. The steel shall conform to specified chemical composition requirements. Rockwell 30T hardness test shall be done to the plates. This test forms the basis for a system of temper designation. The mechanical properties of continuously annealed plate and batch annealed plate of the same Rockwell 30T temper designation are not identical. It is important to keep in mind, that the Rockwell 30T test does not measure all various factors which contribute to the fabrication characteristics of the plate.
Область применения1.1 This specification covers a group of common requirements which, unless otherwise specified in the purchase order or in an individual specification, shall apply to tin mill products.
1.2 The following safety hazards caveat pertains to Annex A1 through Annex A8 of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Note 1—This metric specification is equivalent to Specification A 623 and is compatible in technical content.