Standard Test Method for Thermal Conductivity of Refractories — 6 стр.
Область применения

1.1 This test method covers the determination of the comparative thermal conductivity of refractories under standardized conditions of testing. This test method is designed for refractories having a conductivity factor of not more than 200 Btu[dot]in./h[dot]ft [dot]°F (2818 W/m[dot]K), for a thickness of 1 in. (25 mm).

1.2 Detailed ASTM test methods to be used in conjunction with this procedure in testing specific types of refractory materials are as follows: Test Method C182, Test Method C202, Test Method C417, and Test Method C767.

1.3 The values stated in inch-pound units are to be regarded as the standard. The values in parentheses are provided for information only.

1.4 This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety problems associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

ICS
81.080 Refractories. Including ceramic refractories / Огнеупоры. Включая огнеупоры из керамики
Сборник ASTM
15.01 Refractories, Activated Carbon; Advanced Ceramics / Огнеупорные материалы; Активированный уголь, Высококачественная керамика
Тематика
Refractories