5.1 Moisture adds mass to the coke and serves no useful purpose. A knowledge of the moisture content is important in the purchase and sale of green petroleum coke, both of which are conducted on a dry basis.
5.2 The collection of the sample as specified for the Drying Oven Method is intended for the express purpose of determining the total moisture of green petroleum coke. The standard is available to producers, sellers, and consumers for determination when other techniques or modifications are not mutually agreed on.
5.3 The Preparation Procedure is used only when sample contains free water. Obtaining a representative sample of a coke source is compounded by the presence of free water.
Область применения1.1 This test method covers both the preparation procedure for samples containing free water (air drying loss (ADL) on gross moisture samples) and the determination of the gross moisture content of green petroleum coke.
1.2 Units—The values stated in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.