The compression resistance perpendicular to the faces, the resistance to the extrusion during compression, and the ability to recover after release of the load are indicative of a joint filler's ability to fill continuously a concrete expansion joint and thereby prevent damage that might otherwise occur during thermal expansion. The asphalt content is a measure of the fiber-type joint filler's durability and life expectancy. In the case of cork-type fillers, the resistance to water absorption and resistance to boiling hydrochloric acid are relative measures of durability and life expectancy.
Область применения1.1 These test methods cover the physical properties associated with preformed expansion joint fillers. The test methods include:
PropertySection Expansion in Boiling Water7.1 Recovery and Compression7.2 Extrusion7.3 Boiling in Hydrochloric Acid7.4 Asphalt Content7.5 Water Absorption7.6 Density7.7Note 1—Specific test methods are applicable only to certain types of joint fillers, as stated herein.
1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.