Standard Specification for High-Strength Low-Alloy Structural Steel Plate with Low Carbon and Restricted Sulfur for Improved Weldability, Formability, and Toughness— 3 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 25 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 27 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 27 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 25 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 26 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf>o</inf></emph>, for Ferritic Steels in the Transition Range— 25 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 25 стр.
Standard Test Method for Determination of Reference Temperature, <emph type="bdit">T<inf >o</inf></emph>, for Ferritic Steels in the Transition Range— 27 стр.
Standard Test Method for Determining Plane-Strain Crack-Arrest Fracture Toughness, <emph type="bdit">K<inf>Ia</inf></emph>, of Ferritic Steels— 20 стр.