4.1 These test methods for the chemical analysis of ferroniobium alloy are primarily intended to test such materials for compliance with compositional specifications such as Specification A550. It is assumed that all who use these test methods will be trained analysts capable of performing common laboratory procedures skillfully and safely. It is expected that work will be performed in a properly equipped laboratory.
Область применения1.1 These test methods cover the chemical analysis of ferroniobium having chemical compositions within the following limits:
Element
Composition, %
Aluminum
2.00 max
Carbon
0.30 max
Chromium
2.00 max
Cobalt
0.25 max
Lead
0.01 max
Manganese
3.00 max
Niobium
40.00 to 75.00
Phosphorus
0.05 max
Silicon
4.00 max
Sulfur
0.03 max
Tantalum
7.00 max
Tin
0.15 max
Titanium
5.00 max
Tungsten
0.50 max
1.2 The test methods appear in the following order:
Sections
Separation of Niobium, Tantalum, and Titanium by the Ion-Exchange Test Method
15 and 16
Titanium by the Spectrophotometric Test Method [0.05 % to 5.0 %]
17 – 21
Niobium by the Gravimetric Test Method [40 % to 75 %]
22 – 23
Tantalum by the Gravimetric Test Method [1 % to 7 %]
24 – 25
Tantalum by the Spectrophotometric Test Method [0.25 % to 1 %]
26 – 30
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific hazard statements are given in Section 6, and specific warning statements in 11.1.