This specification covers requirements for the compound and physical characteristics of rubber floor tile. The polymeric binder of the rubber floor tile shall have been vulcanized such that it becomes thermoset. The rubber floor tile made from this compound shall be resistant to neutral pH cleaners. For homogeneous rubber floor tile, the surface coloring or mottling shall be uniform throughout the entire thickness of the rubber floor tile. For layered rubber floor tile, the surface color or mottling need not extend through the entire thickness of the rubber floor tile, but must extend throughout the entire thickness of the wear layer. The material shall be tested for heat resistance, abrasion resistance, dimensional stability, and light resistance.
Область применения1.1 This specification covers requirements for the compound and physical characteristics of rubber floor tile.
1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.
1.3 The following precautionary statement applies only to the test method portion, Section 7, of this specification. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.