Testing of Elastomers - Determination of Indentation Hardness of Soft Rubber (IRHD), Hardness Testing on Specimens of Small Dimensions, Micro-testing— 2 стр.
Glass in building - Determination of the bending strength of glass - Part 3: Test with specimen supported at two points (four point bending); German version EN 1288-3:2000— 7 стр.
Glass in building - Determination of the bending strength of glass - Part 3: Test with specimen supported at two points (four point bending); German version EN 1288-3:2000— 7 стр.
Testing of glass and glass ceramics; determination of bending strength; coaxial double ring bending test on flat specimens with small test area— 6 стр.
Testing of glass and glass ceramics; determination of bending strength; coaxial double ring bending test on a flat test piece with large test area— 12 стр.