This document specifies the conditions for determination of tensile properties of ceramic matrix composite
materials with continuous fibre reinforcement for temperatures up to 2 000 °C under vacuum or a gas
atmosphere which is inert to the material under test.
NOTE The use of these environments is aimed at avoiding changes of the material to be tested due to chemical
reaction with its environment during the test.
This document applies to all ceramic matrix composites with a continuous fibre reinforcement, unidirectional
(1D), bidirectional (2D), and tridirectional (xD, with 2 < x <= 3), loaded along one principal axis of reinforcement.
Diese Europäische Norm legt die Bedingungen zur Bestimmung der Eigenschaften von endlosfaserverstärkten keramischen Verbundwerkstoffen unter Zugbelastung bei Temperaturen bis zu 2 000 °C im Vakuum oder in einer gegenüber dem Probenwerkstoff inerten Gasatmosphäre fest. Diese Europäische Norm gilt für alle endlosfaserverstärkten Verbundwerkstoffe mit keramischer Matrix mit unidirektionaler (1D), bidirektionaler (2D) und tridirektionaler (xD, mit 2 < x <= 3) Verstärkung mit der Belastung entlang einer der Hauptverstärkungsachsen.