This International Standard specifies a method for the determination of the linear density of all types of yarn in package form, with the exception of any yarn that may be the subject of a separate International Standard. It includes seven optional procedures based on different methods of conditioning and preparation (see 4.1 and 4.2). Since the different procedures do not give the same values, it is essential that the procedure used is agreed by all Parties interested in the test results. While this method is designed solely for the determination of mass per unit length of yarn, it is frequently desirable to combine this determination with tests for
strength and/or tests for commercial mass. If, in such a case, skein lengths other than those specified are used, the length used, and any special corrections based on it, are subject to agreement between the interested Parties. This method is applicable to
a) Single yarns (spun, monofilament or multifilament);
b) folded (plied) yarns;
c) cabled yarns.
It is not applicable, except by agreement, to yarns which stretch more than 0,5 % when the tension, in centinewtons, per unit linear density of yarn, in tex, increases from 0,5 to l,O. Such yarns may be tested under special conditions if they are accepted by all the
Parties interested in the test results. The method is not applicable to yarns having a linear density greater than 2 000 tex. For such yarns, other skein lengths and special conditions of reeling may
be adopted by agreement of the interested Parties.
Diese ÖNORM legt Methoden zur Bestimmung der Feinheit sämtlicher Garntypen von Aufmachungseinheiten fest, mit Ausnahme jener Garne, die Gegenstand einer gesonderten ÖNORM sein können. Sie enthält sieben Verfahren zur wahlweisen Anwendung auf der Grundlage unterschiedlicher Arten der Konditionierung und Vorbereitung sowie unterschiedlicher Vorgaben. Da die verschiedenen Verfahren nicht zu gleichen Werten führen, ist es wesentlich, daß das anzuwendende Verfahren von allen an den Prüfergebnissen interessierten Parteien angenommen wird. Die Methoden sind anwendbar auf- Einfachgarne (Spinnfasergarn, monofiles oder multifiles Filamentgarn); - mehrfache (einstufige) Zwirne; - mehrstufige Zwirne. Die Methoden sind nicht anwendbar auf Garne, die sich um mehr als 0,5 % dehnen, wenn die feinheitsbezogene Vor- spannkraft von 0,5 cN/tex auf 1,0 cN/tex erhöht wird. Sie sind auch nicht anwendbar auf Garne mit einer Feinheit über 2000 tex.