SAE AMS4902G
Заменен
Titanium Sheet, Strip, and Plate Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
Описание
Изменения
Ссылки
Версии
Ссылочные документы
SAE AMS2242G
Действует
Tolerances Corrosion and Heat Resistant Steel, Iron Alloy, Titanium, and Titanium Alloy Sheet, Strip, and Plate
SAE AMS2249J
Действует
Chemical Check Analysis Limits Titanium and Titanium Alloys
SAE AMS2750H
Действует
Pyrometry
SAE AMS2809B
Действует
Identification, Titanium and Titanium Alloy Wrought Products
ASTM E112-96e3
Заменен
Standard Test Methods for Determining Average Grain Size
— 26 стр.
ASTM E1209-99
Заменен
Standard Test Method for Fluorescent Liquid Penetrant Examination Using the Water-Washable Process
— 6 стр.
ASTM E1409-97
Заменен
Standard Test Method for Determination of Oxygen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
— 4 стр.
ASTM E1447-92(1996)
Заменен
Standard Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Thermal Conductivity Method
— 3 стр.
ASTM E290-97a(2004)
Заменен
Standard Test Methods for Bend Testing of Material for Ductility
— 7 стр.
ASTM E384-99e1
Заменен
Standard Test Method for Microindentation Hardness of Materials
— 24 стр.
ASTM E8M-04
Заменен
Standard Test Methods for Tension Testing of Metallic Materials [Metric] (Withdrawn 2008)
— 24 стр.
SAE MAM2242D
Действует
Tolerances, Metric, Corrosion and Heat Resistant Steel, Iron Alloy, Titanium, and Titanium Alloy Sheet, Strip, and Plate
SAE AMS4902H
Заменен
Titanium Sheet, Strip, and Plate Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
SAE AMS4902F
Заменен
TITANIUM SHEET, STRIP, AND PLATE Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
На этот документ ссылаются
SAE AMS4902H
Заменен
Titanium Sheet, Strip, and Plate Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength
SAE AMS4902F
Заменен
TITANIUM SHEET, STRIP, AND PLATE Commercially-Pure Annealed 40.0 ksi (276 MPa) Yield Strength